| performance | test condition | unit | Copper plate insulation special material |
| specificities | Flame retardant, weather resistant, highly insulating | ||
| temperature rating | ℃ | 105 | |
| durometer | ShoreA | 92±2 | |
| proportion | g/cm3 | 1.3 | |
| Elongation before aging | 50mm/min | % | 270#100 |
| Tensile strength before aging | 50mm/min | Mpa | 16.8#10.3 |
| ageing condition | 135±2℃*240HRs | ||
| Elongation after aging | % | 250 | |
| Maximum change in elongation after aging | % | 6.3 | |
| Tensile strength after aging | 50mm/min | Mpa | 16.2 |
| Maximum rate of change of tensile strength after aging | 50mm/min | % | 3.6 |
| Heat Resistance Test | 135±2℃*240HRs | non-laminated | |
| Low Temperature Impact Test | -15 | ℃ | PASS |
| volume resistance | 23±1℃ | Ω.m | 8.2*1014 |
| Flame retardant grade | UL94 V-0 | mm | 2.5 |
| Processing Information | ℃ | 155~175 |